Св-13Х25Н18
Mark Св-13Х25Н18

High-alloy welding wire Св-13Х25Н18 made in accordance with GOST 2246-70.
Application
Dissimilar critical structures, different types of steel, as well as products which can be operated in the temperature. to 1000C in oxidizing environments. Fields of application are mechanical engineering, chemical, food and oil industry.
Chemical composition
|
Element |
Cr |
Ni |
Mn |
Si |
P |
С |
S |
|
Content, % |
24-26,5 |
17-20 |
1-2 |
0,5 |
0,025 |
0,15 |
0,015 |
Mechanical properties of the wire Sv-13H25N18:
Toughness – KCV – 150 J / cm2;
Tensile strength – 635 MPa;
Elongation – 32%;
Tensile strength – 475 MPa.